| Bronze Bushing LG2 |
| Typical Composition |
|
Min. |
Max. |
| |
Copper |
84% |
86% |
| Tin |
4% |
6% |
| Zinc |
4% |
6% |
| Lead |
4% |
6% |
| Phosphorus |
|
.05% |
| Aluminium |
|
.005% |
| Related Specifications |
| |
AS C83600 AS.1565-1985 C83600 |
| BS.1400 LG2 |
| ASTM 836 |
| SAE 40 |
| Available in continuous cast bar and hollow sections, see stocked sizes. |
| Bronze Bushing AB1 (Aluminium Bronze) |
| Typical Composition |
|
Min. |
Max. |
| |
Copper |
86.00% |
|
| Tin |
|
0.10% |
| Zinc |
|
0.50% |
| Nickel |
|
1.00% |
| Lead |
|
0.05% |
| Aluminium |
8.50% |
9.50% |
| Iron |
2.50% |
4.00% |
| Manganese |
|
1.00% |
| Related Specifications |
| |
AS1565-1985 C95210 |
| B.S. 1490 AB1 |
| A.S.T.M. 952 |
| S.A.E. 68A/68B |
| Used where corrosion resistance is required such as marine, oil or chemical industries |
| |
Colour Code |
Silver End |
| Bronze Bushing PB1 (Phosphour Bronze) |
| Typical Composition |
|
Min. |
Max. |
| |
Copper |
Remainder |
|
| Tin |
10.20% |
12.00% |
| Zinc |
|
0.05% |
| Nickel |
|
0.10% |
| Lead |
|
0.25% |
| Phosphorous |
|
1.20% |
| Aluminium |
|
0.005% |
| Iron |
|
0.10% |
| Related Specifications |
| |
A.S.T.M. 1565-1985 904D |
| B.S. 1490 PB1 |
| S.A.E. 65 |
| Commonly used for gears, bearings and heavy load bushes. |
| |
Colour Code |
Yellow End |
| Bronze Bushing PB2 (Phosphour Bronze) |
| Typical Composition |
|
Min. |
Max. |
| |
Copper |
Remainder |
|
| Tin |
11.20% |
13.00% |
| Zinc |
|
0.30% |
| Nickel |
|
0.50% |
| Lead |
|
0.25% |
| Phosphorous |
0.15% |
0.80% |
| Aluminium |
|
0.005% |
| Iron |
|
0.15% |
| Manganese |
|
1.00% |
| Related Specifications |
| |
A.S. 1565-1985 907C |
| B.S. 1490 PB2 |
| S.A.E. 65 |
| Commonly used for gears, worm wheels and where shock resistance is required |
| |
Available subject to enquiry |
| Other grades are available subject to enquiry. |